Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | 0.000 °C | 32.0 °F | |
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |
|||
Clash Berg Stiffness Temperature | 0.000 °C | 32.0 °F | |
Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |