Polymer Property : Ring & Ball Softening Point = 112 °C
Polymer Property :
Ring & Ball Softening Point =
112 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Ring & Ball Softening Point
104
-
112
°C
219
-
234
°F
542-112
Westlake Epolene® N-11P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Information provided by Westlake Chemical