Thermal Properties Metric English Comments
Ring & Ball Softening Point 166 °C
331 °F
ASTM E28
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co..