Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 78.0 °C
172 °F
ASTM E28
Arkema Group EVATANE® 33-400 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-400 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-400 is stabilized with antioxidants. The High Vinyl Acetate ..