Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 99.0 °C | 210 °F | ASTM E28 |
DuPont Elvax® 420 Ethylene Vinyl Acetate DuPont™ Elvax® 420 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 420 resins can be used for the following applications: adhesives, sealants.. |