Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 223 °C | 433 °F | ASTM E28 |
DuPont Elvax® 470 Ethylene Vinyl Acetate DuPont™ Elvax® 470 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 470 resins can be used for the following applications: .. |