Thermal Properties | Metric | English | Comments |
---|---|---|---|
Ring & Ball Softening Point | 112 - 145 °C | 234 - 293 °F | Average value: 130 °C Grade Count:4 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |