Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 200 °C
>= 392 °F
Arkema Group OREVAC® 9314 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..