Polymer Property : Ring & Ball Softening Point = 43.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Ring & Ball Softening Point 35.0 - 43.0 °C
95.0 - 109 °F
Unipetrol 160/220 Road Bitumen
At normal temperatures, road bitumens are semi-solid to solid homogeneous bitumen substances. They are produced as residual fractions of vacuum distillation of the atmospheric crude oil residual fra..