Thermal Properties Metric English Comments
Ring & Ball Softening Point >= 37.0 °C
>= 98.6 °F
after aging @ 163°C
Unipetrol 160/220 Road Bitumen
At normal temperatures, road bitumens are semi-solid to solid homogeneous bitumen substances. They are produced as residual fractions of vacuum distillation of the atmospheric crude oil residual fra..