Thermal Properties Metric English Comments
Transformation Temperature 540 °C
1000 °F
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Transformation Temperature 540 °C
1000 °F
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca..
Transformation Temperature 540 °C
1000 °F
Ferro IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates)
Typical Powder Form: TF Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can..