Thermal Properties Metric English Comments
Transformation Temperature 749 °C
1380 °F
Ac<sub>3</sub>
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
An oil-hardening alloy with excellent size change properties, Stentor tool steel is especially suited for general purpose work in the toolroom. It is safe to harden, and shows little size change or ..