Thermal Properties Metric English Comments
Transformation Temperature 138 - 143 °C
280 - 289 °F
Temp at Max Expansion
Akzo Nobel Expancel® 007 WUF 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 138 - 146 °C
280 - 295 °F
Temp at Max Expansion
Akzo Nobel Expancel® 053 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 138 - 146 °C
280 - 295 °F
Temp at Max Expansion
Akzo Nobel Expancel® 053 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 138 - 148 °C
280 - 298 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Transformation Temperature 138 - 148 °C
280 - 298 °F
Expansion Starting Temperature
Akzo Nobel Expancel® 950 DU 120 Dry unexpanded microspheres