Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 455 °C | 851 °F | |
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |