Thermal Properties Metric English Comments
Transformation Temperature 600 °C
1110 °F
Ferro EG 2778 Thick Film Glass
Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..
Transformation Temperature 600 °C
1110 °F
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a..