Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 730 °C
1350 °F
Ac<sub>1</sub>
Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6)
R.D.S. tool steel is an oil hardening die steel which combines extreme toughness with very little size change when heat treated. It is available as a DeCarb-Free product. DCF bars have been cold fin..