Polymer Property : Transformation Temperature = 857 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature 857 °C
1570 °F
Ac<sub>1</sub>
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 538°C (1000°F)
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Transformation Temperature 857 °C
1570 °F
Ac<sub>1</sub>
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Transformation Temperature 857 °C
1570 °F
Ac<sub>1</sub>
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 593°C
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Transformation Temperature 857 °C
1570 °F
Ac<sub>1</sub>
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Transformation Temperature 857 °C
1570 °F
Ac<sub>1</sub>
Carpenter Pyrotough® 78 Hot Work Die Steel
Pyrotough® 78 alloy is a premium quality hot work die steel engineered to withstand the operating temperatures and pressures associated with die casting and hot extrusion operations. The patented c..