Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = -1.50 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point <= -1.50 °C
<= 29.3 °F
BASF Epsilon-Caprolactone
Formula: C6H10O2CAS: 502-44-3Description: Epsilon-caprolactone is a colorless to yellow liquid, with a perceptible odor. It is soluble in water.Synonyms: 6-Hydroxyhexanoic acid lactone, Caprolacton..
Melting Point -1.50 °C
29.3 °F
BASF N4-Amine N,N’-Bis-(3-Aminopropyl)ethylene-diamine
Formula: C8H22N4CAS: 10563-26-5Description: N4 Amine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 4,7-Diazadecane-1,10-diamine, 1,5,8,12-Tetraazadodeca..
Melting Point -1.50 °C
29.3 °F
BASF N4-Amine S N,N'-Bis-(3-Aminopropyl)ethylene-diamine
Formula: C8H22N4CAS: 10563-26-5Description: N4-Amine S is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1,3-Propanediamine,N,N”-1,2-ethanediylbis- 1,5,8,1..