Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -90.0 °C | -130 °F | Freezing Point |
LG Chemical 2-Ethyl Hexyl Acrylate Features: Low Color- Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity -Through the multistage .. |
|||
Melting Point | <= -90.0 °C | <= -130 °F | |
Solvay Chemicals TAB Tert-Amylbenzene Tert-Amylbenzene is a chemical intermediate.. Tert-pentylbenzene: CAS-No.: 2049-95-8 / EC-No.: 218-076-0 /REACH Registration Number: 01-2119450079-38Uses: Chemical intermediate and Laboratory chemi.. |
|||
Melting Point | -90.0 °C | -130 °F | Freezing Point |
BASF 2- Ethylhexyl Acrylate Formula: C11H20O2CAS: 203-080-7Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. .. |