Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | -130.5 °C | -202.9 °F | n-Pentane |
LG Chemical IP-20 Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o.. |
|||
Melting Point | -130.5 °C | -202.9 °F | n-Pentane |
LG Chemical IP-40 Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o.. |