Melting Point -95.0 °C
-139 °F
LG Chemical Toluene
Colorless liquid with benzene odor, Heavier than air and highly inflammable, and Not soluble to water, Readily soluble in alcohol and etherStructure & Characteristics: C6H5CH3. Synthesized by extrac..