Thermal Properties Metric English Comments
Melting Point -15.0 °C
5.00 °F
Freezing Point
Solvay Chemicals 1,2,3-Trichloropropane
Colourless liquid, mainly used as chemical intermediate.EINECS Number: 202-486-1/CAS Number: 96-18-4/UN number: 2810Information provided by Solvay
Melting Point -15.0 °C
5.00 °F
Solvay Chemicals Trifluoroacetic acid
Fluorinated Acids CAS-No.: 76-05-1 / EC-No.: 200-929-3 / Index-No.: 607-091-00-1 Uses: Solvent, Chemical intermediate and CatalystInformation provided by Solvay
Melting Point -15.0 °C
5.00 °F
Shandong Dongyue Polymer TFP Tetrafluoropropanol
Usage: TFP is widely used on medicine, agrichemical, dyestuff and intermediate of fine chemical such as the color agent of photography, textile finishing agent, fluoropolymer assistant ingredient, d..
Melting Point <= -15.0 °C
<= 5.00 °F
Freezing Point
Solvay TOLCIDE® PS 70A 70% tetrakis hydroxymethyl phosphonium sulfate
Identification: CONCENTRATE BASED UPON TETRAKIS(HYDROXYMETHYL)PHOSPHONIUM SULPHATE (THPS) AND A BIOPENETRANTCAS: 55566-30-8Function: Concentrate for formulation into TOLCIDE® PS70A, PS50A & PS20A..
Melting Point <= -15.0 °C
<= 5.00 °F
Freezing Point
Solvay Amyl Acid Phosphate
Identification: AMYL ACID PHOSPHATE - Phosphoric acid, mono – and bis –(branched and linear pentyl esters)CAS: 84418 – 71 – 3Available in: Asia Pacific, Europe, Latin America and..