Polymer Property : Melting Point = -53.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point -53.0 °C
-63.4 °F
Freezing Point
LG Chemical DIDP Plasticizer
Features: LG anti-static ABS AP-163 has been developed through the unique technologies. This product shows superior electrical insulating properties.Application: Sheet, power cableInformation provid..