Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= -7.00 °C | <= 19.4 °F | |
Dow Corning 2-2617 Diesel Antifoam 100% active polysilicone polyether copolymer, used to control foam in diesel fuel.Information provided by Dow Corning |
|||
Melting Point | -7.00 - -1.00 °C | 19.4 - 30.2 °F | |