Thermal Properties Metric English Comments
Melting Point -80.0 - 130 °C
-112 - 266 °F
Average value: 40.0 °C Grade Count:4
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Melting Point -80.0 °C
-112 °F
Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP
Non Ozone depleting, VOC exempt, Silicone cleaner to clean Plastic and Metals, excellent for removing oils, silicone-based car wax and protectants.Information provided by Dow Corning
Melting Point <= -80.0 °C
<= -112 °F
BASF Ethyl Chloroformate
Formula: C3H5ClO2CAS: 541-41-3Description: Ethyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Chloroformic acid ethyl ester..
Melting Point <= -80.0 °C
<= -112 °F
BASF N-Methylpyrrolidine
Formula: C5H11NCAS: 120-94-5Description: N-Methylpyrrolidine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Methylpyrrolidin, N-Methyltetrahydropyrr..
Melting Point -80.0 °C
-112 °F
BASF Propionaldehyde
Formula: C3H6OCAS: 123-38-6Description: Propionaldehyde is a colorless liquid, with a pungent odor. It is miscible in water in all proportions and is soluble in other organic solvents.Synonyms: Prop..