Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1024 °C | 1875 °F | |
American Elements Neodymium Nanoparticles General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec.. |