Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 20.0 - 40.0 °C | 68.0 - 104 °F | |
BASF Lupragen® DMI 1,2-Dimethyl Imidazole Formula: C5H8N2CAS: 1739-81-0Description: 1,2-Dimethylimidazole is a colorless to yellowish solid with an amine-like odor. Synonyms: DMI, 1,2-Dimethyl-1H-imidazolApplications: It is used as a Cataly.. |