Polymer Property : Melting Point = 1078 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1063 - 1078 °C
1945 - 1972 °F
Williams Advanced Alloys Wambraze™ WB1078 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TB Quenched Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TB Quenched Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD1 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD2 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD3 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD3 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TDX Quenched/Cold Rolled, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TF Quenched/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH2 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH2 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Melting Point 968 - 1078 °C
1770 - 1972 °F
CLAL-MSX NICLAFOR® 1000 THX Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..