Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 43.0 °C
109 °F
ASTM D3418
Parker Chomerics THERMFLOW T443
THERMOFLOW phase-change materials are specially formulated for use in high performance devices requiring minimum thermal resistance for maximum component reliability. The major advantage of using TH..
Melting Point 43.0 - 53.0 °C
109 - 127 °F
Fine Organics FINALUX G 602 Lubricant Additive
Applications: Universal internal lubricant for rigid PVC and foamed PVC, applicable independently of stabilizing system. Pseudo-plasticizer for PVC. Low improver and lubricant for PMMAInformation ..
Melting Point 43.0 °C
109 °F
Solvay ANTAROX® PL 122 Surfactant
Description: General purpose dispersing agent.Chemical Name: ETHYLENE/PROPYLENE OXIDE BLOCK POLYMERCAS: 9003 – 11 – 6Solubility Dispersible in water. Soluble in most polar and aromatic sol..
Melting Point 43.0 °C
109 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® N416 Polymer Modifier
Fusabond® N416 is a chemically modified ethylene elastomer. Used as a polymer modifier Fusabond N416 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the ..