Polymer Property : Melting Point = 1100 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 593 °C
1100 °F
Heatbath/Park Pen Karb Deepcase Carburizer
Cyanide Liquid Carburizer. Stable, barium-energized, liquid deep case carburizing salt producing carbon case depths ranging up to .100 inches. Provides equal or better case characteristics than gas..