Thermal Properties Metric English Comments
Melting Point 1102 - 1120 °C
2016 - 2050 °F
Universal Wire Works Au-Pd-Ni (AMS 4784) Gold Brazing Filler Metal
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Melting Point 1102 - 1121 °C
2016 - 2050 °F
Williams Advanced Alloys Wambraze™ WB1121 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..