Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1107 - 1150 °C | 2025 - 2100 °F | |
Universal Wire Works BCo-1 (AMS 4783) Nickel Base Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |