Thermal Properties Metric English Comments
Melting Point 45.0 - 55.0 °C
113 - 131 °F
Fine Organics FINALUX G 722 Lubricant Additive
Applications: Compatible external lubricant for rigid PVC fittings, bottles, films and sheets.Information provided by Fine Organics
Melting Point 45.0 - 55.0 °C
113 - 131 °F
Struktol V-PEDS Processing Additive
Fatty acid esterTypical Applications: STRUKTOL® V-PEDS has both internal and external lubricant characteristics. It can be used in calendaring, extrusion and injection molding applications. It al..
Melting Point 45.0 °C
113 °F
ASTM D3418 - ISO 3146
DuPont Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melting Point 45.0 °C
113 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3180 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
28 wt% Vinyl Acetate.Elvax® 3180 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melting Point 45.0 °C
113 °F
Freezing Point; ASTM D3417
DuPont Elvax® 3180Z Ethylene Vinyl Acetate
DuPont™ Elvax® 3180Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicati..