Thermal Properties Metric English Comments
Melting Point 1138 - 1220 °C
2080 - 2220 °F
Kennametal Stellite Delcrome® 93
Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high..