Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1175 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 635.0 °C
1175 °F
Heatbath/Park Sta-Hard 17 High Speed Hardening Salt
A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu..
Melting Point 635.0 °C
1175 °F
Heatbath/Park Sta-Hard 17 Neutral Salt
A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatu..
Copyright © lookpolymers.com All Rights Reserved