Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 122 °C | 252 °F | Internal method |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Melting Point | 122 °C | 252 °F | Exxon Method |
ExxonMobil Escorene® LL-6101 LLDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, High Gloss, Excellent ImpactUses: Large houseware containers, General purpose injection molding |
|||
Melting Point | 122 °C | 252 °F | Exxon Method |
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Melting Point | 122 °C | 252 °F | DSC; ASTM D3418 |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 122 °C | 252 °F | DSC |
Silon Tabond 3044 Adhesive Resin TABOND 3044 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Str.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D3418 |
Westlake Tymax™ GA4402 Anhydride Modified Linear Low Density Polyethylene (Developmental Resin) Westlake GA4402 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5100.09 Compounding Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5252.09 Compounding Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045G Linear Low Density Polyethylene DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2078G Linear Low Density Polyethylene Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2267G Linear Low Density Polyethylene A high performance stretch film resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9064 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9064 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Internal Measurement |
Bapolene® 83 Polyethylene Terephthalate Applications: Personal care, household, liquor and food containers. All data is based on molded plaques. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
Lushan M-10F Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melting Point | 122 °C | 252 °F | |
M. Holland Company MAGMA® LM115-C LLDPE
(discontinued **) Additives: Medium Antiblock, Low SlipFeatures: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |