Polymer Property : Melting Point = 127.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point <= 127.2 °C
<= 261.0 °F
DSC; Lyondell Test
LyondellBasell Alathon® L4434 High Density Polyethylene
ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet..