Thermal Properties Metric English Comments
Melting Point 54.4 °C
130 °F
Dow Method (DSC)
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ..