Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 603 - 705 °C | 1120 - 1300 °F | |
Indium Corp. Indalloy 179 Silver Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 680 - 705 °C | 1260 - 1300 °F | |
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing Optimum Joint Gap 0.1 - 0.25 mm.AWS A5.8-92 BAg-22BS EN 1044 1999 AG502Equivalent to Engelhard Silvaloy A-49NMEquivalent to Handy & Harman Braze 495Information provided by Johnson Matthey. |
|||
Melting Point | 660 - 705 °C | 1220 - 1300 °F | |
Johnson Matthey Argo-braze 502 Silver Brazing Alloy for Tungsten Carbide Brazing These products are specifically designed for brazing of tungsten carbide tips to steel tools and wear parts. Optimum Joint Gap 0.1 - 0.25 mm.AMS 4788AWS A5.8-92 BAg-24Equivalent to Engelhard Silvalo.. |
|||
Melting Point | 640 - 705 °C | 1180 - 1300 °F | |
Indium Corp. Indalloy 211 Ag-Cu Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 630 - 705 °C | 1170 - 1300 °F | |
Williams Advanced Alloys Wambraze™ WB705 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |