Polymer Property : Melting Point = 1305 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1305 - 1375 °C
2381 - 2507 °F
Special Metals NIMONIC® Alloy 81
A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content o..