Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 131.2 °C | 268.2 °F | ASTM D3418 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Melting Point | 131.2 °C | 268.2 °F | ASTM D3418 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |