Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1310 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 605 - 710 °C
1120 - 1310 °F
Indium Corp. Indalloy 212 Ag-Cu-Zn-Cd Solder Alloy
Information Provided by Indium Corporation
Melting Point 670 - 710 °C
1240 - 1310 °F
Johnson Matthey Argo-braze 49LM Silver Brazing Alloy for Tungsten Carbide Brazing
This material is supplied as Trifoil. Trifoil consists of a layer of copper sandwiched by brazing alloy. The copper helps to absorb the stresses caused by the differential expansion rates, under he..
Melting Point 650 - 710 °C
1200 - 1310 °F
Johnson Matthey Matti-sil 40Sn Cadmium Free Brazing Alloy
A general purpose alloy, often used for refrigeration work.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-28BS EN 1044 1999 AG105Equivalent to Engelhard Silvaloy A-40TEquivalent to Handy & Harman ..
Melting Point 607.2 - 710 °C
1125 - 1310 °F
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy
Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai..
Melting Point 649 - 710 °C
1200 - 1310 °F
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy
Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative..
Melting Point 607.2 - 710 °C
1125 - 1310 °F
Lucas-Milhaupt EASY FLO 30 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 30 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue ..
Melting Point 649 - 710 °C
1200 - 1310 °F
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 402 is a free-flowing, intermediate temperature filler metal and as such is a good substitute for cadmium-bearing filler metals with similar silver contents. The material is ..
Copyright © lookpolymers.com All Rights Reserved