Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1350 - 1400 °C | 2470 - 2560 °F | |
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel INCOLOY alloy 25-6HN is a super-austenitic stainless steel containing 6% molybdenum and with properties enhanced by its content of nitrogen. Its high content of nickel results in thermal stability .. |
|||
Melting Point | 1350 °C | 2460 °F | |
Goodfellow Aluminum 50/Nickel 50 Alloy Information provided by Goodfellow. |
|||
Melting Point | 1350 °C | 2462 °F | |
California Fine Wire Stablohm 675 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Melting Point | 1350 - 1413 °C | 2470 - 2575 °F | |
Carlson C 600 Nickel-Chromium-Iron Alloy Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c.. |
|||
Melting Point | 1350 - 1413 °C | 2470 - 2575 °F | |
Carlson C 600ESR Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell.. |
|||
Melting Point | 1350 °C | 2460 °F | |
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |