Polymer Property : Melting Point = 1360 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 516 - 738 °C
961 - 1360 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Melting Point 516 - 738 °C
961 - 1360 °F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Melting Point 675 - 735 °C
1250 - 1360 °F
Johnson Matthey Matti-sil 45 Cadmium Free Brazing Alloy
A medium flowing alloy which is often used for marine and Shipbuilding applications.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-5BS EN 1044 1999 AG203Federal Specification QQ-B-564 BAg-5Equival..
Melting Point 690.6 - 738 °C
1275 - 1360 °F
Lucas-Milhaupt BRAZE 700 (Medium) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..