Polymer Property : Melting Point = 14.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 13.0 - 14.0 °C
55.4 - 57.2 °F
BASF N-Vinyl-2-pyrrolidone, Non-Stabilized
Formula: C6H9NOCAS: 88-12-0Description: Vinyl pyrrolidone is a colorless to yellowish liquid, with a characteristic odor. It is miscible in water and organic solvents.Synonyms: N-Vinylpyrrolidone, ..
Melting Point 12.0 - 14.0 °C
53.6 - 57.2 °F
BorsodChem ONGRONAT T 80 TDI 80/20 Isocyanate
Description of product:Appearance: At room temperature water clear liquid. Composition: A mixture of toluene-di-isocyanate isomers (2,4-toluene-di-isocyanate [A] and 2,6-toluene-di-isocyanate [B].No..