Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 743 - 760 °C | 1370 - 1400 °F | |
Williams Advanced Alloys Wambraze™ WB760 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |