Thermal Properties Metric English Comments
Melting Point 1370 - 1430 °C
2500 - 2610 °F
Pyramid Stainless Steel AISI 304/316L, STAINLESS STEEL SHEET NO.4 FINISH
Information provided by Pyramid Stainless Steel Ind Co Ltd
Melting Point 1400 - 1430 °C
2550 - 2610 °F
Kennametal Stellite Denertiaâ„¢ C14 Cobalt Chromium Dental Alloy
Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §..
Melting Point 1370 - 1430 °C
2500 - 2610 °F
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy
Data provided by the manufacturer, Special Metals.
Melting Point 1395 - 1430 °C
2543 - 2610 °F
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
Melting Point 1390 - 1430 °C
2530 - 2610 °F
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
Melting Point 1390 - 1430 °C
2530 - 2610 °F
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Melting Point 1230 - 1430 °C
2250 - 2600 °F
Crucible Steel 321 Chromium-Nickel Steel
Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe..
Melting Point 1370 - 1430 °C
2500 - 2610 °F
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at ..