Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical EM500 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical EM500A Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical EM600A Impact modifier for Engineering Plastics LG Chem impact modifiers for Engineering Plastics are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modifiers - Buta.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical IM810 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical MB802 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical MB838A Opaque impact modifier Description: MBS type opaque impact modifiers from LG Chem are appropriate for improving impact strength all the PVC products of rigid and semi-rigid opaque PVC, and have differentiated characterist.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical MB872 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical MB885 Transparent impact modifier Description: MBS type transparent impact modifiers from LG Chemical is used to improve impact strength and processability of PVC products, and classified into transparent grade and low chlorosis gra.. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical PA910 Processing aid Description: General purposeApplication: Sheet, window profile, pipe etcInformation provided by LG Chemical |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical EM600 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Melting Point | 148 - 149 °C | 298 - 300 °F | |
AIM 80In/Pb15/Ag5 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 132 - 149 °C | 270 - 300 °F | |
LG Chemical IM812 Acrylic impact modifier Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for pro.. |