Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 1620 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 880 - 900 °C
1620 - 1650 °F
Wieland 1605 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental
Melting Point 880 - 975 °C
1620 - 1790 °F
Williams Advanced Alloys Wambraze™ WB975 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..
Melting Point 880 °C
1620 °F
Goodfellow Copper 80/Tin 20 Alloy
Information provided by Goodfellow.