Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 900 - 960 °C | 1650 - 1760 °F | |
Wieland 1103 Wilaform Gold Hard yellow gold alloy particularly suitable for decoration casting.Applications: casting, laminar decorationDental |
|||
Melting Point | 900 - 915 °C | 1650 - 1680 °F | |
Wieland 1914 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Melting Point | 900 - 950 °C | 1650 - 1740 °F | |
Williams Advanced Alloys Wambraze™ WB950 Solder High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de.. |
|||
Melting Point | 900 - 1050 °C | 1650 - 1920 °F | |
Goodfellow Phosphor Bronze Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow. |
|||
Melting Point | 899 °C | 1650 °F | |
Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed bor.. |